On Friday, I wrote about the development of amorphous or “glassy” metal alloys, in which the atoms are packed together with no regular crystal structure. At the microscopic level, almost all metals are made of crystal grains, which can be bigger or smaller depending on how the metal has been heat treated. Amorphous alloys, recall, are extremely unusual among metals because they can be cast without forming crystal grains at all.
At the opposite end of the spectrum are single crystal (SC or SX) alloys, which are mixtures of metals that can be cast in such a way that the entire object is essentially a single giant “grain,” i.e. one continuous crystal. Among minerals like quartz, large objects composed of a single crystal are fairly common; you also may have seen the large ingots of artificially-grown single-crystal silicon, known as “boules,” from which wafers are cut to make microchips and other semiconductor devices.

But when it comes to metals, single-crystal objects are outside of most people’s experience. Forming single-crystal metal objects requires both special alloys and special casting techniques. The alloys are almost always nickel-based, with as many as nine minor metal components including five or more percent chromium, cobalt, tungsten, tantalum, aluminum, and/or rhenium. The casting method is known as “directional solidification,” and involves carefully cooling a cast metal part starting at one end to guarantee a particular orientation of its crystal structure. That orientation is chosen, naturally, based on expected stresses in the finished part.
The primary application for single crystal superalloys is the manufacture of jet engine turbine blades, which must endure tremendous forces at extremely high temperatures for prolonged periods of time. Under such conditions, metals with a grain structure tend to “creep,” or slowly deform, along grain boundaries. Because single-crystal alloy parts have no grain boundaries, however, they are highly resistant to this kind of wear.
If you’re interested in reading more, check out the excellent online primer on nickel-based superalloy technology maintained by The University of Cambridge’s Dr. Harry Bhadeshia.










Someday, I want to be SMR smrt…
I was actually given one of these turbine blades when I was visiting an air-force base (it was a “dead” one, removed from an engine during overhaul). The tech’s spent a wee while explaining the process in creating them, and that they are single-cyrtal metals…
Fascinating stuff, and I have a piece of single-crystal metal as a souvenir! I’d almost forgotten about it until I saw that previous post and dug it out…
I don’t know, it’s probably a burden being that smart. You have to suffer the likes of dumb guys like us.
Pingback: Information by ccurtis - Pearltrees
Pingback: MAKE | Top 10: Marvellous Metals
Pingback: Top 10: Marvelous Metals | vis a vis | visual mind
// What's Trending
Raspberry Pi Design Contest
Dad Builds Son an Iron Man Arc Reactor
Teardrop Camper Trailer
Seventeen Sneaky Secret Hides
What to do with an 800 Lb Eucalyptus Slab
10 Things to Connect to Your Raspberry Pi
3D Printed Kinetic iPhone Cases
80-Ruxpin Art Installation
// What's Shared
A better way to slice a pumpkin
DIY Nerf Darts
100 Dollar Store Organization Ideas for Craft Rooms and Beyond
In the Maker Shed: Minty Boost USB Charger
Mad’s Mouse House
Lace Princess Crowns
I Have a (Puzzling) Dream
Play the Rings of a Tree Trunk Like a Record
// Most Commented
Plastic Bags into Plastic Blocks: Revisited
10 Hot New Boards to Watch
Why the Maker Movement is Here to Stay
MAKE Asks: Roadside Hacks
Ten Tips for Hand Saws and Blades
DIY Hacks & How To’s: Convert From Battery Power to AC
How To Make Your Own Laundry Detergent
What to do with an 800 Lb Eucalyptus Slab